Rilsan? BESVOA MED
聚酰胺 11
Arkema
产品说明:
Rilsan ? BESVOA MED is a polyamide produced from a renewable source. This natural grade, dedicated to extrusion, contains a negligible amount of oligomers. Rilsan ? BESVOA MED offers the highest quality and it is specifically designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request letters regarding USP Class VI compliance can be provided.
MAIN APPLICATIONS
物理性能 | 额定值 | 单位制 | 测试方法 |
---|
密度 | 1.02 | g/cm? | *** 1183 |
硬度 | 额定值 | 单位制 | 测试方法 |
---|
肖氏硬度 |
|
| *** 868 |
邵氏 D | 76 |
| *** 868 |
邵氏 D, 15 秒 | 71 |
| *** 868 |
机械性能 | 额定值 | 单位制 | 测试方法 |
---|
拉伸模量 | 1180 | MPa | *** 527-2 |
拉伸应力 |
|
| *** 527-2 |
屈服 | 36.0 | MPa | *** 527-2 |
断裂 | 52.0 | MPa | *** 527-2 |
拉伸应变 |
|
| *** 527-2 |
屈服 | 5.0 | % | *** 527-2 |
断裂 | > 200 | % | *** 527-2 |
弯曲模量 | 1100 | MPa | *** 178 |
冲击性能 | 额定值 | 单位制 | 测试方法 |
---|
简支梁缺口冲击强度 |
|
| *** 179 |
-30°C | 13 | kJ/m? | *** 179 |
23°C | 15 | kJ/m? | *** 179 |
简支梁无缺口冲击强度 |
|
| *** 179 |
-30°C | 无断裂 |
| *** 179 |
23°C | 无断裂 |
| *** 179 |
热性能 | 额定值 | 单位制 | 测试方法 |
---|
熔融温度 | 186 | °C | *** 11357-3 |
补充信息 | 额定值 | 单位制 | 测试方法 |
---|
*** Shortname | PA11, E, 22-010 |
| *** 1874 |
Renewable Carbon Conent | 100 | % | ASTM D6866 |
挤出 | 额定值 | 单位制 |
|
---|
干燥温度 | 65.0 到 80.0 | °C |
|
干燥时间 | 4.0 到 6.0 | hr |
|
熔体温度 | 230 到 280 | °C |
|